Stainless Steel / 17-4 PH COND H-1150

17-4 material is provided in the H1150 heat treat condition to make the material softer than the annealed condition. The material is baked at 1150 degrees for four hours and then air cooled to obtain a tensile strength of 135 - 170 ksi.

Chemical Makeup

Element Min Max
Carbon, C 0.07
Manganese, Mn 1
Silicon, Si 1
Sulfur, S 0.03
Phosphorus, P 0.04
Chromium, Cr 15 17.5
Molybdenum, Mo - 0.5
Nickel, Ni 3 5
Columbium (Niobium), Nb 5xC 0.45
Copper, Cu 3 5

Common Applications

  • Aerospace Aerospace
  • Medical Medical
  • Industrial Industrial

Benefits

  • Good Corrosion Resistance
  • Formability & Weldability
  • High Strength & Hardness

We stock 17-4 PH COND H-1150 to the following specifications:

  • ASTM-A-564
  • CHEMS TO AMS-5643
  • ASTM F-899