A-286 1650 Solution Treated is a nickel and iron-based austenitic superalloy that is solution annealed at 1650 and then precipitation heat treated (aged) to provide a minimum room temperature tensile strength of 140 KSI. This alloy is useful for parts requiring moderate strength up to 1300 F (704 C) and oxidation resistance up to 1500 F (816 C). A-286 material has wide applications in high temperature fasteners, springs, jet engine components, offshore oil and gas turbines. (UNS S66286)
Element | Min | Max |
---|---|---|
Carbon, C | -- | 0.08 |
Manganese, Mg | -- | 2 |
Silicon, Si | -- | 1 |
Phosphorus, P | -- | 0.025 |
Sulfur, S | -- | 0.025 |
Chromium, Cr | 13.5 | 16 |
Nickel, Ni | 24 | 27 |
Molybdenum, Mo | 1 | 1.5 |
Titanium, Ti | 1.9 | 2.35 |
Boron, B | 0.003 | 0.01 |
Vanadium, V | 0.1 | 0.5 |
Cobalt, Co | -- | 1 |
Aluminum, Al | -- | 0.35 |
Copper, Cu | -- | 0.5 |